Opens in a new tab

How to Prevent Creasing on PCBs After Assembly?

Published: November 4, 2026 · Updated: November 4, 2026

In the PCB (Printed Circuit Board) manufacturing process, the flatness of the copper foil is critical to the quality of the final product. If the copper foil is not laid flat, it can cause wrinkling, which may affect the performance and reliability of the circuit board. This article will discuss how to prevent creasing in PCB copper foil to ensure high-quality circuit board manufacturing.

Advanced: What Actually Happens During the Pressing Process?

To understand warping, one must first understand the lamination process. In the lamination of multilayer boards, the inner core layers, prepreg (PP), and copper foil are stacked together, and under high temperature and pressure, the resin melts, flows, and eventually cures into a single, integrated unit:

The key conclusion is:Wrinkles can only occur within the window during which the resin is in a flowing state.. Once the resin gel cures, the position of the copper foil is fixed. Therefore, all anti-wrinkle measures essentially involve controlling the relative displacement of the copper foil within this window.

  • The heating rate determines the window length: The faster the temperature rises, the shorter the flow window;
  • Pressure determines the direction of flow: Uneven pressure can cause the resin to move laterally along with the copper foil;
  • The load plate determines the constraint strength: The tighter the restraint, the less likely the copper sheet is to slip.

Hydraulic Press

For key points on the lamination process, seeLamination Process: The Heart of High-Layer-Count PCB Manufacturing; See "Prepregs and Laminates"The Difference Between Dry Film and Wet Film for PCB Inner Layers。

Copper Foil Flatness and PCB Quality

The flatness of a PCB is critical to its performance and reliability. The copper layer is the conductive layer of the PCB, responsible for connecting the various components and circuits. If the copper layer becomes wrinkled, it may lead to the following series of problems:

  1. Welding Issues: Crumpled copper foil may cause poor soldering, affecting the quality and stability of the solder joints.
  2. Signal IntegrityQuestion: Creases in the copper foil may cause discontinuities in the signal lines, thereby affecting signal transmission.
  3. Electrical Performance Issues: Creases may cause a decline in the electrical performance of the circuit board, including changes in resistance and capacitance.
  4. Reliability Issues: Creases can reduce the reliability of a circuit board and shorten its service life.

Therefore, maintaining the flatness of the copper foil is critical to the quality of the PCB.

Advanced: Even Copper Distribution—The Most Important Consideration in Design

The original text mentions that “one side with a large copper area and the other with a large empty area” is most prone to wrinkles; the principle behind this isLateral Variations in Resin Flow:

  • Large Copper Surface Area: The resin has nowhere to go and is trapped between the copper surfaces, with virtually no flow;
  • Large Open Area: Resin accumulates in large quantities and flows laterally, generating a strong lateral thrust;
  • Boundary: A sudden change in the flow state occurs in these two areas, causing the copper sheet to be squeezed and crumpled here.

The solution was clear right from the design phase:Distribute the copper as evenly as possible. The three most common techniques are:

  1. Add balanced copper: Fill in any open areas with copper blocks or mesh that are not electrically connected to ensure uniform copper coverage;
  2. Switch to grid copper: Replacing large copper areas with a grid pattern preserves the shielding effect while improving resin flow;
  3. Adjust the stacking order: Ensure that the copper distribution in adjacent layers is complementary to avoid overlapping empty areas at the same location.

Note in Article 1: The balancing copper must beNo network connection, and it does not form an antenna structure with other copper tracesisolated copper blocks, and avoid high-speed signal areas; otherwise, new signal integrity issues may arise.

Copper Foil: The Lifeline of PCBs

For precautions regarding copper-clad laminates, see8 Things to Keep in Mind When Applying Copper to a PCB; For copper foil specifications, seeCopper Foil: The Lifeline of PCBs。

Causes of Creases in Copper Foil

There may be several causes for creasing in copper foil. Here are some common causes:

1. Issues with Blank Areas on the Substrate

If there are issues with the blank areas of the PCB substrate—specifically, if excessive flow occurs during the reflow process—this can lead to poor support for the copper layer and an increased likelihood of slippage. Most PCB manufacturers are mindful of routing issues on the inner layers and try to avoid making empty areas too conspicuous. Creasing typically occurs in areas with significant differences in trace density, especially where one side is designed with a large copper pad while the other side has a large empty area.

2. Film Lamination Methods and Hot Pressing Parameters

The choice of film and hot-pressing parameters can also affect wrinkling in the copper foil. If the film layers shift during lamination or if the adhesive flows improperly, the copper foil will drift on the surface of the molten resin, inevitably causing wrinkles. To prevent such issues, the design of the carrier plate used for pressing is critical. Currently, many manufacturers use carrier plates featuring an elastic, height-adjustable anti-slip design. This design completely prevents the steel plate from slipping during the pressing process, thereby reducing the occurrence of wrinkling.

3. Choosing Film

When selecting film, avoid types with excessively high adhesive content whenever possible, and use a lower heating rate during lamination—as long as complete filling is ensured. Choosing the appropriate film type and parameters can reduce the occurrence of wrinkles.

Advanced: Selecting Preforms and Pressing Parameters

The original text emphasizes avoiding the use of film with excessively high resin content precisely because it results in excess flowing resin.The principle for selecting films is to “fill the slot just right” rather than “the more, the better.”: Insufficient adhesive can result in gaps and voids, while excessive adhesive increases the risk of sagging and wrinkles; both extremes should be avoided.

Thick Copper Board

For the characteristics of thick copper boards, see8 Things to Keep in Mind When Applying Copper to a PCB; For challenges related to pressing, seeChallenges in the Manufacturing of High-Layer-Count Printed Circuit Boards and Control of Key Processes。

How to Prevent Creasing in PCB Copper Cladding

To prevent creasing of the copper foil on PCBs, here are some practical tips:

1. Design the circuit board appropriately

When designing a PCB, you should avoid leaving excessively large empty areas on the blank sections of the substrate, especially when one side is designed with a large copper plane while the other side has a large empty area. A proper trace layout can help reduce the occurrence of creasing.

2. Select an Appropriate Substrate Design

In the PCB manufacturing process, selecting an appropriate carrier design is crucial. A slide-stop design with adjustable elastic height can effectively prevent steel plate misalignment and reduce the occurrence of wrinkling.

3. Consider Your Choice of Film

When selecting film, avoid types with excessively high adhesive content, and ensure that film overlap during movement and adhesive flow do not cause the copper foil to shift.

4. Control the hot-pressing parameters

Properly control the hot-pressing parameters, including temperature and pressure, to ensure good adhesion between the molten resin and the copper foil and to minimize the occurrence of wrinkles.

5. Regularly inspect the manufacturing process

Regularly inspect the manufacturing process, including how the film layers are stacked and the condition of the trays. Identifying problems early and taking corrective action can reduce the risk of wrinkling.

Advanced: Platter Design and Device Status

The pressing pallets (steel plates and trays) determine the interlayer constraint conditions. The elastic anti-slip design mentioned in the original text is intended to prevent lateral slippage of the laminate during the pressing process:

  • Steel Plate Flatness: Deformation of the steel plate can cause an uneven distribution of pressure, which directly leads to localized wrinkling;
  • Anti-slip structure: Limiting lateral displacement of the laminate is the most direct way to prevent wrinkling;
  • Cushioning Material: The condition of the cushion pads affects the uniformity of pressure distribution; they must be replaced regularly;
  • Aligning Stacked Boards: The misalignment between layers during stacking is itself a source of displacement.

There are two key points to consider regarding the equipment: the uniformity of the hot plate temperature and the effectiveness of the vacuum system.Uneven temperatures can cause the viscosity of the resin to vary across different areas....Insufficient vacuum causes volatile components to remain in the material and form bubbles; both of these factors exacerbate wrinkling and voids.

  1. Regularly check the temperature distribution of the hot plate: Identify deviations and correct them promptly;
  2. Replace the cushioning material regularly: Judge based on the number of uses, not on appearance;
  3. Record the pressing parameters for each batch: To provide a basis for tracing exceptions.

Thick-Copper PCBs

For issues related to the lamination of multilayer boards, seeCauses and Solutions for Bubbles in the Layers of Multilayer Printed Circuit Boards; For warpage standards, seeStandards and Test Methods for PCB Warpage。

Conclusion

Creasing issues in PCB copper foil can seriously affect the performance and reliability of circuit boards; therefore, manufacturers and designers need to take measures to prevent these problems from occurring. Key steps to reduce warping include proper substrate design, selecting an appropriate carrier design, careful film selection, controlling hot-pressing parameters, and regularly inspecting the manufacturing process. By implementing these measures, high-quality PCB manufacturing can be ensured.


Advanced: How to Distinguish Between Creases, Layers, and Bubbles

The corrective measures for these four types of defects differ; when evaluating cross-sections, determine the type first before taking action. It is worth noting that they sometimes occur simultaneously—for example, insufficient resin filling can result in voids and also cause wrinkles due to localized pressure imbalances.

  • Preliminary Assessment by Visual Inspection and Tactile Examination: Creases are usually visible on the surface;
  • Slice Verification: Determine whether the issue is related to interlayer adhesion or copper foil displacement;
  • Ultrasound Scan: Suitable for batch inspection of interlayer adhesion.

Three Causes of Copper Strip Delamination on PCBs

See the effects on signal integritySignal Integrity Issues in PCB Design; For key points on reliability, seeKey Points on the Reliability of 19 Printed Circuit Boards and Microsectioning Techniques。

Frequently Asked Questions

1. How does the wrinkling of the copper foil on a PCB affect the performance of the circuit board?

Copper foil wrinkling can lead to soldering issues, signal integrity problems, electrical performance issues, and reliability problems, thereby affecting the performance and reliability of the circuit board.

2. Why do blank areas on the substrate cause wrinkling?

Problems with blank areas on the substrate may cause excessive flow during the melting process, resulting in poor support for the copper foil and causing it to slip, which increases the likelihood of wrinkling.

3. How does the carrier plate design affect copper foil wrinkling on a PCB?

A properly designed carrier plate can prevent the steel sheet from slipping and reduce the occurrence of wrinkles.

4. How do I choose the right film?

Avoid using film types with excessively high adhesive content whenever possible, and ensure that lamination movement and adhesive flow do not cause the copper foil to shift.

5. Why is it important to control hot-pressing parameters?

Controlling the hot-pressing parameters ensures good adhesion between the molten resin and the copper foil, thereby reducing the occurrence of wrinkles.

If you need more information or have any other questions, please feel free to contact us.

6. Are thin sheets more prone to wrinkling?

Yes. The copper foil and core material in thin-gauge multilayer boards have lower rigidity and are more easily displaced during resin flow. Therefore, thin-gauge multilayer boards place higher demands on lamination parameters, substrate condition, and uniform copper distribution; particular care must be taken during design to avoid large empty areas.

7. Does balancing copper affect electrical performance?

It is possible. Balancing copper is an isolated copper area; if placed near high-speed signals, it can create parasitic coupling and alter the local impedance. Therefore, balancing copper should be kept as far away as possible from critical high-speed traces and RF areas, and sufficient spacing should be maintained.

8. Can the lamination parameters be used universally?

No. The optimal parameters vary depending on the material system, stack-up, and sheet thickness. When introducing new materials, lamination tests should be conducted to determine the parameter window; simply reusing old parameters is a common cause of batch defects.

9. Can creases be detected during subsequent processing steps?

In most cases, yes. Severe creases can be detected during a visual inspection, while minor ones require a cross-section or ultrasound scan. Therefore, in addition to visual inspection, conducting random cross-section sampling of high-risk batches is a necessary measure.

10. What is the most effective thing a designer can do?

Ensure even copper distribution. This is the most cost-effective and impactful measure; it only requires a single inspection of copper distribution after the wiring is complete, followed by adding additional copper in open areas to achieve balance. In contrast, adjusting parameters during the lamination stage is a reactive measure.

11. Can a panel with creases be repaired?

Generally, no. The wrinkles that form after lamination indicate that the interlayer structure has already cured and set, and cannot be restored by relaminating. Therefore, boards with this type of defect must be scrapped, which is why lamination is considered one of the highest-risk processes in multilayer board manufacturing.

Further Reading:Signal Integrity Issues in PCB Design · 10 Signal Integrity Issues in High-Speed PCB Design